đTYPES OF STAIRS: @COTMp
.
âśDepending upon the various arrangement of steps, stairs can be classified under following categories:
1. STRAIGHT STAIR:
In this stair, all the steps are arranged continuously
along in one direction. One flight may be split into
one or more than one flight by interposing a
landing. This stair can be used where narrow and
long space is available for a staircase such as
entrance, porch etc.
2. DOGGED-LEGGED STAIR:
This stair consists of two straight flights of steps
with direct turns between them. This stair is very
useful where the total width of the stair is just twice
the width of the steps.
3. OPEN NEWEL STAIR:
This type of stair consists of two or more flights
arranging a well or opening between the backward
and forward flights. When all the steps are difficult
to arrange in two flights, a short third flight of 3 to
6 steps may be provided along the direction
perpendicular to the hall. Open newel stair is mostly
adopted in the lift.
4. GEOMETRICAL STAIR:
This is another type of open newel stair where the
open well between the forward and the backward
flight is curved. This stair may contain different
geometrical shape. Here the change in direction is
achieved by using winders.
5. CIRCULAR STAIR:
In this type of stair, all the steps radiate from a
newel or well hole, in the form of winders. The
circular stair is adopted at the back side of a
building to access its various floors.
6. SPIRAL STAIR:
Spiral stair is very similar to a circular stair. It
consists of individual steps or treads, connecting to
a centre column. The overall diameter of the stair
may range from 1 to 2.5 m.
7. QUARTER-TURN STAIR:
The quarter-turn stair can be defined as the stairs
that are turned at 90 degrees with the help of level
landing.
8. BIFURCATED STAIR:
This type of stair is provided in modern public
buildings as well as residential buildings. In this
stair, the flight is so arranged that there is a wide
flight at the start which is sub-divided into narrow
flights at the mid-landing. The narrow flights start
from either side of the mid landing.
.
đŠJoin for more Discussion @COTMA
đđđđđđ
@COTMA @COTMA @COTMA
.
âśDepending upon the various arrangement of steps, stairs can be classified under following categories:
1. STRAIGHT STAIR:
In this stair, all the steps are arranged continuously
along in one direction. One flight may be split into
one or more than one flight by interposing a
landing. This stair can be used where narrow and
long space is available for a staircase such as
entrance, porch etc.
2. DOGGED-LEGGED STAIR:
This stair consists of two straight flights of steps
with direct turns between them. This stair is very
useful where the total width of the stair is just twice
the width of the steps.
3. OPEN NEWEL STAIR:
This type of stair consists of two or more flights
arranging a well or opening between the backward
and forward flights. When all the steps are difficult
to arrange in two flights, a short third flight of 3 to
6 steps may be provided along the direction
perpendicular to the hall. Open newel stair is mostly
adopted in the lift.
4. GEOMETRICAL STAIR:
This is another type of open newel stair where the
open well between the forward and the backward
flight is curved. This stair may contain different
geometrical shape. Here the change in direction is
achieved by using winders.
5. CIRCULAR STAIR:
In this type of stair, all the steps radiate from a
newel or well hole, in the form of winders. The
circular stair is adopted at the back side of a
building to access its various floors.
6. SPIRAL STAIR:
Spiral stair is very similar to a circular stair. It
consists of individual steps or treads, connecting to
a centre column. The overall diameter of the stair
may range from 1 to 2.5 m.
7. QUARTER-TURN STAIR:
The quarter-turn stair can be defined as the stairs
that are turned at 90 degrees with the help of level
landing.
8. BIFURCATED STAIR:
This type of stair is provided in modern public
buildings as well as residential buildings. In this
stair, the flight is so arranged that there is a wide
flight at the start which is sub-divided into narrow
flights at the mid-landing. The narrow flights start
from either side of the mid landing.
.
đŠJoin for more Discussion @COTMA
đđđđđđ
@COTMA @COTMA @COTMA
đSLUMP TEST OF CONCRETE @COTMp
~~~~~~~~~~~~~~~~
âśThe concrete slump test is an empirical test that
measures the workability of fresh concrete. The test
is performed to check the consistency of freshly
mixed concrete in a specific batch. *Consistency refers to the ease and homogeneity with which the concrete can be mixed, placed, compacted and finished. *This test is most widely used due to the simplicity of apparatus and simple test procedure.
*The slump test gives satisfactory results for the
concrete mix of medium to high workability and
unfortunately, it does not give the correct indication
of low workability, which may give zero slumps.
This test is also known as slump cone test.
âśAPPARATUS FOR CONCRETE SLUMP TEST:
1. Mould or slump cone with a height of 300 mm,
bottom diameter 200 mm, and top diameter 100
mm.
2. Standard tamping rod.
3. Non-porous base plate.
4. Measuring scale.
âśPROCEDURE OF TEST:
1. First, clean the inner surface of the empty mould and then apply oil to it.
2. Set the mould on a horizontal non-porous and
non-absorbent base plate.
3. Fill the mould fully by pouring freshly mixed
concrete in three equal layers.
4. Stroke each layer 25 times with the standard
tamping rod over the cross section.
5. After stroking 25 times the top layer is struck off
level, now lift the mould slowly in the vertical
direction without disturbing the concrete cone.
6. Use the measuring scale to measure the difference level between the height of the mould and the concrete sample.
*The subsidence of concrete is known as the slump and the value of slump is measured in mm.
âśTYPES OF SLUMP:
*True Slump: The concrete mass after the test when
slumps evenly all around without disintegration is
called the true slump.
*Shear Slump: When one-half of the concrete mass
slide down the other is called the shear slump. This type of slump is obtained in a lean concrete mix.
*Collapse Slump: When the sample is collapsed due to adding excessive water, it is known as collapse slump.
*Zero Slump: For very stiff or dry mixes it does not
show any changes of the slump after removing the
slump cone.
âśADVANTAGES OF CONCRETE SLUMP TEST:
1. The procedure of slump test is simple and easy
than any other workability test.
2. Inexpensive and portable apparatus are required
for this test.
3. Slump test can be performed at the construction site as well as in the laboratory.
âśLIMITATIONS OF CONCRETE SLUMP TEST:
1. The slump test is limited to concretes with the
maximum size of aggregate less than 38 mm.
2. The test is suitable only for concretes of medium
or high workabilities (i.e having slump values of 25
mm to 125 mm).
3. For very stiff mixes having zero slumps, the
slump test does not show any difference in concretes of different workabilities.
*Recommended Values Of Slumps For Different
Concrete Mixes:
âśTypes Of Concrete Slump Range In mm
1. Heavy mass construction 25-50
2. Pavements 20-30
3. Bridge deck 25-75
4. Beams and slabs 50-100
5. Columns, retaining
walls and thin vertical members etc. 75-150
6. Vibrated concrete 12-25
.
đŠáźá á ááá áááá áĽááłááľá˘
~~~~~~~~~~~~~~~~
âśThe concrete slump test is an empirical test that
measures the workability of fresh concrete. The test
is performed to check the consistency of freshly
mixed concrete in a specific batch. *Consistency refers to the ease and homogeneity with which the concrete can be mixed, placed, compacted and finished. *This test is most widely used due to the simplicity of apparatus and simple test procedure.
*The slump test gives satisfactory results for the
concrete mix of medium to high workability and
unfortunately, it does not give the correct indication
of low workability, which may give zero slumps.
This test is also known as slump cone test.
âśAPPARATUS FOR CONCRETE SLUMP TEST:
1. Mould or slump cone with a height of 300 mm,
bottom diameter 200 mm, and top diameter 100
mm.
2. Standard tamping rod.
3. Non-porous base plate.
4. Measuring scale.
âśPROCEDURE OF TEST:
1. First, clean the inner surface of the empty mould and then apply oil to it.
2. Set the mould on a horizontal non-porous and
non-absorbent base plate.
3. Fill the mould fully by pouring freshly mixed
concrete in three equal layers.
4. Stroke each layer 25 times with the standard
tamping rod over the cross section.
5. After stroking 25 times the top layer is struck off
level, now lift the mould slowly in the vertical
direction without disturbing the concrete cone.
6. Use the measuring scale to measure the difference level between the height of the mould and the concrete sample.
*The subsidence of concrete is known as the slump and the value of slump is measured in mm.
âśTYPES OF SLUMP:
*True Slump: The concrete mass after the test when
slumps evenly all around without disintegration is
called the true slump.
*Shear Slump: When one-half of the concrete mass
slide down the other is called the shear slump. This type of slump is obtained in a lean concrete mix.
*Collapse Slump: When the sample is collapsed due to adding excessive water, it is known as collapse slump.
*Zero Slump: For very stiff or dry mixes it does not
show any changes of the slump after removing the
slump cone.
âśADVANTAGES OF CONCRETE SLUMP TEST:
1. The procedure of slump test is simple and easy
than any other workability test.
2. Inexpensive and portable apparatus are required
for this test.
3. Slump test can be performed at the construction site as well as in the laboratory.
âśLIMITATIONS OF CONCRETE SLUMP TEST:
1. The slump test is limited to concretes with the
maximum size of aggregate less than 38 mm.
2. The test is suitable only for concretes of medium
or high workabilities (i.e having slump values of 25
mm to 125 mm).
3. For very stiff mixes having zero slumps, the
slump test does not show any difference in concretes of different workabilities.
*Recommended Values Of Slumps For Different
Concrete Mixes:
âśTypes Of Concrete Slump Range In mm
1. Heavy mass construction 25-50
2. Pavements 20-30
3. Bridge deck 25-75
4. Beams and slabs 50-100
5. Columns, retaining
walls and thin vertical members etc. 75-150
6. Vibrated concrete 12-25
.
đŠáźá á ááá áááá áĽááłááľá˘
đOPC VS PPC cement @COTMp
.
âśPPC: PPC or Portland Pozzolan's Cement is a mixture of Pozzolan's panic material with Argillaceous and Calcareous materials in powdered form. *Pozzolan's increases the strength of the cement but initial setting time is more than OPC.
*Pozzolan's should be in the range of 10â30%. If more than this range
then strength will be reduced.
*It is useful for most
Civil construction works like mass concreting etc. It
is economical for projects as less cost of cement
than OPC. Gypsum is used for controlling of setting
time.
âśADVANTAGES OF PPC:
1. Higher durability of concrete structure due to less permeability of water.
2. More resistance towards the attack of alkalies,
sulfates, chlorides, chemicals.
3. Better workability.
4. Low heat of hydration.
5. Due to high fineness, PPC has better cohesion
with aggregates and makes more dense
concreteness.
6. Comparative lower Water-Cement ratio provides an added advantage for the further increase of compressive strength of the concrete.
7. Better surface finish.
.
âĄOPC: OPC or Ordinary Portland Cement is a mixture of Calcareous materials with Argillaceous material in
proportional ratio. Gypsum is used for controlling
the setting time. It has less setting time than PPC.
It is useful where work to be complete soon. It is
costlier than PPC. It is available in various grades
such 33, 43 & 53. OPC grade 43 is very useful
nowadays.
âśADVANTAGES OF OPC:
1. Produces highly durable and sound concrete due
to very low percentage of alkalis, chlorides,
magnesia and free lime in its composition.
2. Almost negligible chloride content results in
restraining corrosion of concrete structure in hostile environments.
3. Significant saving in cement consumption while
making concrete of grades M15, M20, M25, M35
and pre-cast segments due to high strength.
âśDIFFERENCE BETWEEN OPC AND PPC:
âĄORDINARY PORTLAND CEMENT (OPC):
1. OPC is produced simply by grinding limestone
and secondary materials to a powder.
*The main raw materials used for manufacturing OPC is calcareous material, argillaceous material, and gypsum.
2. The durability of OPC is lower than PPC.
3. The setting time is of OPC is less than PPC.
4. Costlier than PPC.
5. Mostly used where fast construction is required.
6. The different grades of OPC are:
*OPC 33 Grade
*OPC 43 Grade
*OPC 53 Grade
.
âśPOZZOLANIC PORTLAND CEMENT (PPC):
1. PPC is a variation of OPC which includes a
mixture of a pozzolanic material which is known to
increase the strength of concrete. The raw materials used for manufacturing of PPC is OPC, gypsum, pozzolanic materials such as fly ash, rice husk ash, volcanic tuffs and pumicites, clay & shale, etc.
2. Mostly used in mass concreting, plaster and
masonry.
3. Durability is high.
4. Setting time is greater than OPC.
5. Curing period is a little higher than OPC.
6. It can be used in all type of construction work.
7. There are no such specific grades of PPC like
OPC.
8. Low cost.
.
đđđđđ
Join for more updates via the link below;
t.me/COTMp
đđđđđ
⥠á ááá Join á áá¨á áĽá ááá°áá áĽá áááŤááľ áá áźá áŤáľááá˘
.
âśPPC: PPC or Portland Pozzolan's Cement is a mixture of Pozzolan's panic material with Argillaceous and Calcareous materials in powdered form. *Pozzolan's increases the strength of the cement but initial setting time is more than OPC.
*Pozzolan's should be in the range of 10â30%. If more than this range
then strength will be reduced.
*It is useful for most
Civil construction works like mass concreting etc. It
is economical for projects as less cost of cement
than OPC. Gypsum is used for controlling of setting
time.
âśADVANTAGES OF PPC:
1. Higher durability of concrete structure due to less permeability of water.
2. More resistance towards the attack of alkalies,
sulfates, chlorides, chemicals.
3. Better workability.
4. Low heat of hydration.
5. Due to high fineness, PPC has better cohesion
with aggregates and makes more dense
concreteness.
6. Comparative lower Water-Cement ratio provides an added advantage for the further increase of compressive strength of the concrete.
7. Better surface finish.
.
âĄOPC: OPC or Ordinary Portland Cement is a mixture of Calcareous materials with Argillaceous material in
proportional ratio. Gypsum is used for controlling
the setting time. It has less setting time than PPC.
It is useful where work to be complete soon. It is
costlier than PPC. It is available in various grades
such 33, 43 & 53. OPC grade 43 is very useful
nowadays.
âśADVANTAGES OF OPC:
1. Produces highly durable and sound concrete due
to very low percentage of alkalis, chlorides,
magnesia and free lime in its composition.
2. Almost negligible chloride content results in
restraining corrosion of concrete structure in hostile environments.
3. Significant saving in cement consumption while
making concrete of grades M15, M20, M25, M35
and pre-cast segments due to high strength.
âśDIFFERENCE BETWEEN OPC AND PPC:
âĄORDINARY PORTLAND CEMENT (OPC):
1. OPC is produced simply by grinding limestone
and secondary materials to a powder.
*The main raw materials used for manufacturing OPC is calcareous material, argillaceous material, and gypsum.
2. The durability of OPC is lower than PPC.
3. The setting time is of OPC is less than PPC.
4. Costlier than PPC.
5. Mostly used where fast construction is required.
6. The different grades of OPC are:
*OPC 33 Grade
*OPC 43 Grade
*OPC 53 Grade
.
âśPOZZOLANIC PORTLAND CEMENT (PPC):
1. PPC is a variation of OPC which includes a
mixture of a pozzolanic material which is known to
increase the strength of concrete. The raw materials used for manufacturing of PPC is OPC, gypsum, pozzolanic materials such as fly ash, rice husk ash, volcanic tuffs and pumicites, clay & shale, etc.
2. Mostly used in mass concreting, plaster and
masonry.
3. Durability is high.
4. Setting time is greater than OPC.
5. Curing period is a little higher than OPC.
6. It can be used in all type of construction work.
7. There are no such specific grades of PPC like
OPC.
8. Low cost.
.
đđđđđ
Join for more updates via the link below;
t.me/COTMp
đđđđđ
⥠á ááá Join á áá¨á áĽá ááá°áá áĽá áááŤááľ áá áźá áŤáľááá˘
Telegram
ETCONp Discussion
đŠáááááá ááłáĽ áĽá á áľá°áŤá¨áľ @Philemona7
âď¸áá ᨠ@etconp áááŤáŤ ááŠááš ááá˘
âThis is discussion group of @ETCONpWORK
.
đááłá°áĽáŤ ...
.
âĄď¸ááŠá áá ááááá ᨠáŽááľáľáŤáá˝á ááłáŽá˝ á᪠ááá á á ááá á ááááľá!
@ETCONpBOT áááá áĽááá°ááááđ
âď¸áá ᨠ@etconp áááŤáŤ ááŠááš ááá˘
âThis is discussion group of @ETCONpWORK
.
đááłá°áĽáŤ ...
.
âĄď¸ááŠá áá ááááá ᨠáŽááľáľáŤáá˝á ááłáŽá˝ á᪠ááá á á ááá á ááááľá!
@ETCONpBOT áááá áĽááá°ááááđ
đBASICS OF CRACKING PROBLEMS: @COTMp
.
âśThe subject â CRACKS â or â CRACKING â in
concrete is indeed much debated. However, there is
inadequate clarity as to the reason for cracking and
what mey be done to limit its occurrence or
eliminate it altogether.
The phenomenon of the appearance of cracks in
concrete is often a subject that raises several
questions. Either at the initial stage or with time,
cracks may appear in a concrete structure. It should
first of all be accepted that cracks of some type or
other are inevitable in any concrete. They can be
minimized to a large extent by proper practices.
Cracks may be big or small, structural or non-
structural. All of them can be a nuisance by way of
either marring the appearance or function as a
passage for atmospheric polluting gases and
moisture to either the body of concrete and causes
distress.
Cracks in the concrete structure do not always
mean that the structure is not useable. As cracking
of concrete is inherent, what really matters is the
type of structure and the nature of cracking. Cracks
that are acceptable for building structures may not
be acceptable for water relating structures.
Considering that cracking xan never be completely
eliminated, it is necessary to be aware of the
causes, evaluation and the methods of repair
whoever required.
CRACKS
Cracks are generally of towtypes : Structural and
non-structural. Cracks can occur in hardened or
unhardened concrete.
STRUCTURAL CRACKS
It is fundamental that hardened reinforced concrete
cracks in the tensile zone when subjected to
externally imposed structural loads. By means of
appropriate design and detailing technique, these
cracks can be limited to acceptable levels in terms
of structural integrity and aesthetics.
NON_STRUCTURAL CRACKS
Concrete is also liable to crack in both the plastic
and hardened states due to the nature of its
constituent materials. These intrinsic cracks are as
inevitable as structural cracks. Ti is often possible
to predict when intrinsic cracks are likely and to
limit them to acceptable levels by means of good
design and/or proper construction techniques.
DORMANT AND LIVE CRACKS:
Cracks caused by shrinkage, temperature gradient
due to hydration and alkali silica reaction ( ASR )
are less dangerous the cracks caused by thermal
expansion and loads. This is because shrinkage
and hydration temperature gradient result in
dormant cracks ( where the width does not vary
with time) and other mechanisms result in live
cracks (where the width increases with time
Dormant cracks, especially narrow ones, are more
likely to undergo autogenous healing and
realkalisation. The crack may heal owing to
following conditions:
⢠carbon dioxide diffusing into the crack leading to
carbonation of the calcium hydroxide and
precipitation of calcium carbonate.
⢠Cement hydration due to presence of moisture.
⢠Hydration diffusing from the bulk concrete into the
heaked zone thereby increasing the pH in that area.
Live cracks are more likely than domant ones. They
result in collection of debris at the base owing to
movement of the sides on the cracks. This can
impede temporarily the passage of depassivating
substances to the reinforcements. However,
autodeneous healing is unlikely with live cracks.
CAUSES OF CRACKING:
Cracking will occur whenever the applied strain
exceeds the tensile strain capacity of the concrete.
The tensile strain capacity of concrete varies with
age and with
Age at which cracks may occur.
Cracks can appear at any time. The age which
some typical can occur are given in the Table.
TABLE â AGE AT WHICH CRACKS MAY APPEAR:
Sr. no. types of cracks Age
1. plastic shrinkage First few minutes or hours after
concreting .
2. plastic settlement First few minutes or hours
after concreting.
3. due to corrosion After one year or many years.
4. due to loads After loads are imposed and the
time duration of loading
5. due to weight Just after formwork support are
removed.đđđ
.
âśThe subject â CRACKS â or â CRACKING â in
concrete is indeed much debated. However, there is
inadequate clarity as to the reason for cracking and
what mey be done to limit its occurrence or
eliminate it altogether.
The phenomenon of the appearance of cracks in
concrete is often a subject that raises several
questions. Either at the initial stage or with time,
cracks may appear in a concrete structure. It should
first of all be accepted that cracks of some type or
other are inevitable in any concrete. They can be
minimized to a large extent by proper practices.
Cracks may be big or small, structural or non-
structural. All of them can be a nuisance by way of
either marring the appearance or function as a
passage for atmospheric polluting gases and
moisture to either the body of concrete and causes
distress.
Cracks in the concrete structure do not always
mean that the structure is not useable. As cracking
of concrete is inherent, what really matters is the
type of structure and the nature of cracking. Cracks
that are acceptable for building structures may not
be acceptable for water relating structures.
Considering that cracking xan never be completely
eliminated, it is necessary to be aware of the
causes, evaluation and the methods of repair
whoever required.
CRACKS
Cracks are generally of towtypes : Structural and
non-structural. Cracks can occur in hardened or
unhardened concrete.
STRUCTURAL CRACKS
It is fundamental that hardened reinforced concrete
cracks in the tensile zone when subjected to
externally imposed structural loads. By means of
appropriate design and detailing technique, these
cracks can be limited to acceptable levels in terms
of structural integrity and aesthetics.
NON_STRUCTURAL CRACKS
Concrete is also liable to crack in both the plastic
and hardened states due to the nature of its
constituent materials. These intrinsic cracks are as
inevitable as structural cracks. Ti is often possible
to predict when intrinsic cracks are likely and to
limit them to acceptable levels by means of good
design and/or proper construction techniques.
DORMANT AND LIVE CRACKS:
Cracks caused by shrinkage, temperature gradient
due to hydration and alkali silica reaction ( ASR )
are less dangerous the cracks caused by thermal
expansion and loads. This is because shrinkage
and hydration temperature gradient result in
dormant cracks ( where the width does not vary
with time) and other mechanisms result in live
cracks (where the width increases with time
Dormant cracks, especially narrow ones, are more
likely to undergo autogenous healing and
realkalisation. The crack may heal owing to
following conditions:
⢠carbon dioxide diffusing into the crack leading to
carbonation of the calcium hydroxide and
precipitation of calcium carbonate.
⢠Cement hydration due to presence of moisture.
⢠Hydration diffusing from the bulk concrete into the
heaked zone thereby increasing the pH in that area.
Live cracks are more likely than domant ones. They
result in collection of debris at the base owing to
movement of the sides on the cracks. This can
impede temporarily the passage of depassivating
substances to the reinforcements. However,
autodeneous healing is unlikely with live cracks.
CAUSES OF CRACKING:
Cracking will occur whenever the applied strain
exceeds the tensile strain capacity of the concrete.
The tensile strain capacity of concrete varies with
age and with
Age at which cracks may occur.
Cracks can appear at any time. The age which
some typical can occur are given in the Table.
TABLE â AGE AT WHICH CRACKS MAY APPEAR:
Sr. no. types of cracks Age
1. plastic shrinkage First few minutes or hours after
concreting .
2. plastic settlement First few minutes or hours
after concreting.
3. due to corrosion After one year or many years.
4. due to loads After loads are imposed and the
time duration of loading
5. due to weight Just after formwork support are
removed.đđđ
6. due to chemical changes in hardened
concrete After one or many years depending in
chemical attack from outside (sulphate ) Or
chemical reaction from within (ASR)
.
âśCRITICAL CRACK WIDTH: The most common reasons for controlling crack
width are following:
APPERANCE : Unsightly cracking should be avoid
since it may cause concern to the occupants of the external structure.
Ti may also contribute to
unsightly staining on exposed external surfaces,
where salts and rust are washed out from the crack.
DURABILITY: Excessively wide cracks may lead to
corrosion of the reinforcement which in turn may lead to spalling of concrete due to the expansive nature of the corrosion process.
WATER-TIGHTNESS: This is of importance in water
retaining structures.
In particular instances there may be other reasons for controlling cracking in addition to the three reasons cited above.
Crack width is, generally, to be taken to mean the
measurable width of a crack at the surface of
concrete. Crack width limitation is important from durability considerations. Most structural codes
prescribe maximum allowed crack widths.
Codes normally consider cracking caused by
external imposed conditions such as live loading
and provide formula for calculating the crack width
in the design phase. Mainly bending and tension or
bending and axial load are considered. The
direction of such cracks is perpendicular to the
direction of the main reinforcement. Plastic
shrinkage cracks follow the line of reinforcement.
According to IS: 456-2000 the surface of the width
of the cracks should not in general exceeds o.3 mm
in members where cracking is not harmful and does
not have any serious effect either on the
preservation of reinforceing steel or on the durability
of the structures.
In members, where cracking of the tensile zone is
harmful either because they are moisture or in
contact with soil or groundwater, an upper limlt of
0.2 mm is suggested.
For aggressive conditions the surface width of
cracks should not generally exceed 0.1 mm. The
crack width conditions the surface width of cracks
should not be generally exceed 0.1 mm. The crack
width is measured at the surface for the above
purposes. However some other codes specify the
width at points near the reinforcement.
.
đŠShare Share Share
concrete After one or many years depending in
chemical attack from outside (sulphate ) Or
chemical reaction from within (ASR)
.
âśCRITICAL CRACK WIDTH: The most common reasons for controlling crack
width are following:
APPERANCE : Unsightly cracking should be avoid
since it may cause concern to the occupants of the external structure.
Ti may also contribute to
unsightly staining on exposed external surfaces,
where salts and rust are washed out from the crack.
DURABILITY: Excessively wide cracks may lead to
corrosion of the reinforcement which in turn may lead to spalling of concrete due to the expansive nature of the corrosion process.
WATER-TIGHTNESS: This is of importance in water
retaining structures.
In particular instances there may be other reasons for controlling cracking in addition to the three reasons cited above.
Crack width is, generally, to be taken to mean the
measurable width of a crack at the surface of
concrete. Crack width limitation is important from durability considerations. Most structural codes
prescribe maximum allowed crack widths.
Codes normally consider cracking caused by
external imposed conditions such as live loading
and provide formula for calculating the crack width
in the design phase. Mainly bending and tension or
bending and axial load are considered. The
direction of such cracks is perpendicular to the
direction of the main reinforcement. Plastic
shrinkage cracks follow the line of reinforcement.
According to IS: 456-2000 the surface of the width
of the cracks should not in general exceeds o.3 mm
in members where cracking is not harmful and does
not have any serious effect either on the
preservation of reinforceing steel or on the durability
of the structures.
In members, where cracking of the tensile zone is
harmful either because they are moisture or in
contact with soil or groundwater, an upper limlt of
0.2 mm is suggested.
For aggressive conditions the surface width of
cracks should not generally exceed 0.1 mm. The
crack width conditions the surface width of cracks
should not be generally exceed 0.1 mm. The crack
width is measured at the surface for the above
purposes. However some other codes specify the
width at points near the reinforcement.
.
đŠShare Share Share
đTYPES OF STAIRS: @COTMp
.
âśDepending upon the various arrangement of steps, stairs can be classified under following categories:
1. STRAIGHT STAIR:
In this stair, all the steps are arranged continuously
along in one direction. One flight may be split into
one or more than one flight by interposing a
landing. This stair can be used where narrow and
long space is available for a staircase such as
entrance, porch etc.
2. DOGGED-LEGGED STAIR:
This stair consists of two straight flights of steps
with direct turns between them. This stair is very
useful where the total width of the stair is just twice
the width of the steps.
3. OPEN NEWEL STAIR:
This type of stair consists of two or more flights
arranging a well or opening between the backward
and forward flights. When all the steps are difficult
to arrange in two flights, a short third flight of 3 to
6 steps may be provided along the direction
perpendicular to the hall. Open newel stair is mostly
adopted in the lift.
4. GEOMETRICAL STAIR:
This is another type of open newel stair where the
open well between the forward and the backward
flight is curved. This stair may contain different
geometrical shape. Here the change in direction is
achieved by using winders.
5. CIRCULAR STAIR:
In this type of stair, all the steps radiate from a
newel or well hole, in the form of winders. The
circular stair is adopted at the back side of a
building to access its various floors.
6. SPIRAL STAIR:
Spiral stair is very similar to a circular stair. It
consists of individual steps or treads, connecting to
a centre column. The overall diameter of the stair
may range from 1 to 2.5 m.
7. QUARTER-TURN STAIR:
The quarter-turn stair can be defined as the stairs
that are turned at 90 degrees with the help of level
landing.
8. BIFURCATED STAIR:
This type of stair is provided in modern public
buildings as well as residential buildings. In this
stair, the flight is so arranged that there is a wide
flight at the start which is sub-divided into narrow
flights at the mid-landing. The narrow flights start
from either side of the mid landing.
.
đŠGo for Conversation
đđđđđ
@COTMA
.
âśDepending upon the various arrangement of steps, stairs can be classified under following categories:
1. STRAIGHT STAIR:
In this stair, all the steps are arranged continuously
along in one direction. One flight may be split into
one or more than one flight by interposing a
landing. This stair can be used where narrow and
long space is available for a staircase such as
entrance, porch etc.
2. DOGGED-LEGGED STAIR:
This stair consists of two straight flights of steps
with direct turns between them. This stair is very
useful where the total width of the stair is just twice
the width of the steps.
3. OPEN NEWEL STAIR:
This type of stair consists of two or more flights
arranging a well or opening between the backward
and forward flights. When all the steps are difficult
to arrange in two flights, a short third flight of 3 to
6 steps may be provided along the direction
perpendicular to the hall. Open newel stair is mostly
adopted in the lift.
4. GEOMETRICAL STAIR:
This is another type of open newel stair where the
open well between the forward and the backward
flight is curved. This stair may contain different
geometrical shape. Here the change in direction is
achieved by using winders.
5. CIRCULAR STAIR:
In this type of stair, all the steps radiate from a
newel or well hole, in the form of winders. The
circular stair is adopted at the back side of a
building to access its various floors.
6. SPIRAL STAIR:
Spiral stair is very similar to a circular stair. It
consists of individual steps or treads, connecting to
a centre column. The overall diameter of the stair
may range from 1 to 2.5 m.
7. QUARTER-TURN STAIR:
The quarter-turn stair can be defined as the stairs
that are turned at 90 degrees with the help of level
landing.
8. BIFURCATED STAIR:
This type of stair is provided in modern public
buildings as well as residential buildings. In this
stair, the flight is so arranged that there is a wide
flight at the start which is sub-divided into narrow
flights at the mid-landing. The narrow flights start
from either side of the mid landing.
.
đŠGo for Conversation
đđđđđ
@COTMA