Forwarded from Deleted Account
What is the name of the chemical sprayed mostly on ground surface before construction starts?
Anonymous Quiz
17%
Weed killer chemical
58%
Anti termite chemical
10%
Anti fungal chemical
14%
Anti algae chemical
It is called an anti termite chemical compound.
Termite control chemical should be sprayed on the ground formation level Before constructing any RC structures.
The sides and bottom surfaces of the ground surface where any RC structures comes in contact with the ground should be sprayed with anti termite chemicals. Termites are very dangerous insects and causes a huge harm on a concrete surface. They create what is called "termite infestation"where by termites form a colony and starts destroying the surface of the concrete.
The chemical used is either chloropyrifos or lindane. It is available in a form of a bottle. The chemical is mixed with water as per the proportion shown in the specification.It is applied at a rate of 5L per meter square.
The major use of applying antitermite chemical is to establish barrier between termites(insects) in the soil and the building.
It keep termites away from the structure or kills those that penetrates the treated area.
But Anti fungal and anti algae paints are applied in a form of a paint directly to the reinforced concrete structure itself. It is applied on walls and ceiling susceptible to fungus.👷♂️✌
Termite control chemical should be sprayed on the ground formation level Before constructing any RC structures.
The sides and bottom surfaces of the ground surface where any RC structures comes in contact with the ground should be sprayed with anti termite chemicals. Termites are very dangerous insects and causes a huge harm on a concrete surface. They create what is called "termite infestation"where by termites form a colony and starts destroying the surface of the concrete.
The chemical used is either chloropyrifos or lindane. It is available in a form of a bottle. The chemical is mixed with water as per the proportion shown in the specification.It is applied at a rate of 5L per meter square.
The major use of applying antitermite chemical is to establish barrier between termites(insects) in the soil and the building.
It keep termites away from the structure or kills those that penetrates the treated area.
But Anti fungal and anti algae paints are applied in a form of a paint directly to the reinforced concrete structure itself. It is applied on walls and ceiling susceptible to fungus.👷♂️✌
Forwarded from Ethio Construction Engineering
➡Hydraulics and water supply Lecture @COTMp
.
👉ለዛሬ ደሞ የ ላየኛው የምድር ውሃ (surface water) ለማጣራት የምንጠቀማቸው ዘዴዎች ኣዘጋጅተናል 👇
.
⓵ስክሪኒንግ (screening) - ይህ የመጀመረርያው የማጣራት
ደረጃ ሲሆን በዚህ የማጣራት ዘዴ ውስጥ በውሃው ላይ የሚንሳፈፉ ግዙፍ አካላትን ለምሳሌ የዛፍ ጉቶ ፣ግንድ፣ ቅጠል እና ልዩ ልዩ የፕላስቲክ ተንሳፋፊ ቁሳቁሶች ወደ ዋናው የማጣሪያ ገንዳ እና ስርዓት
እንዳይገቡ ያግዳል ።
.
⓶ማርጋት (Coagulation )፦ በዚህ የማጣራት ደረጃ ላይ
ለአይን እይታ ያነሱ ጥቃቅን
አካላትን (Particle size 10^-7cm የሚሆኑ) በማርጋት እና
የኬሚካል ቻርጃቸውን ኒውትራላይዝ የሚያረግ ኬሚካል በመጨመር እርስ በእርሳቸው
እንዲሳሳቡ ማድረግ ነው ።
ለዚህ የአልሙኒየም ፖሊመሮች (Alum) እና አይረን (Fe+3)
አገልግሎት ላይ ይውላሉ።
እንደ የቁልቋል ተክል ያሉ የተፈጥሮ አርጊዎች (coagulants) መጠቀምም ይቻላል
.
⓷ጉግለት (Flocculation)፦ ይህ እርከን ፤ ማርጋት
(coagulation ) ወቅት የረጉ ጥቃቅን አካላትን እርስ በእርሳቸው ቦንድ እስኪፈጥሩ እና እርስ በእርሳቸው ተጣብቀው እስኪጓግሉ ውሃው በተለያየ ፍጥነት የሚማሰልበት ነው።
ይህ ዘዴ ሜካኒካል ወይም ማኑዋል በሆነ መልኩ ይተገበራል።
.
⓸መዝቀጥ/ማዝቀጥ (sedimentation) ፦ በፍሎኩሌሽን ወቅት የጓጎለው ጥቃቅን አካላት በዚህን የማጣራት ደረጃ እንዲዘቅጡ ይደረጋል ። ይህ ዘዴ የሚተገበረው የሚጣራው የውሃን ፍጥነት በመቀነስ ግራቪቲን ተጠቅሞ እንዲዘቅጥ ማድረግ ነው።
በግራቪቲ ለማዝቀጥ የሚከብዱ እጅግ ጥቃቅን ቆሻሻዎችን በፍሎኩሌሽን ወቅት ስንጠቀማቸው የነበሩ ኬሚካሎችን በመጠቀም እንዲዘቅጡ ይደረጋል።
.
⓹ ማጥራት (filtration ) ፦ በዚህ የማጥራት ደረጃ ከማዝቀጥ
ደረጃ ያለፉ ጥቃቅን ቆሻሻዎችን እጅግ ጥቃቅን ቀዳዳዎች ባሉት አካል (medium ) እንዲያልፍ በማድረግ የድፍረስነቱን መጠን እጅግ መቀነስ ነው።
.
⓺ማከም (Disinfection) ፦ ከላይ በተጠቀሱ የማጣሪያ ሂደቶች የተጣራው ውሃ
(በዋነኛነት ከተለያዩ ህይወት ከሌላቸው ጥቃቅን ቆሻሻዎች)
ለህብረተሰቡ ለአገልግሎት
ከመድረሱ በፊት በዚህ ሂደት (ዲስኢንፌክሽን) ማለፍ አለበት ።
ምክንያቱም ውሃው ለአገልግሎት የሚቀርበው ከተለያዩ በአይን ከማይታዩ በሽታ አምጪ ተህዋስያን ነፃ መሆኑ ሲረጋገጥ ነው ። ዲስኢንፌክሽን ውሃውን በማፍላት ፣ ሚካኒካል
በሆነ መልኩ ፣ ለጨረር በማጋለጥ (radiation ) እንደሁም በኬሚካል ሊከናወን ይችላል።
በሃገራችን በዋነኛነት
ሃሎጅኖችን (ብሮሚን ክሎሪን እና አይኦዲን ) በመጠቀም
ኬሚካል በመጠቀም ውሃን እናክማለን ።
፟
➡ከዚህ ሁሉ የማጣራት ሂደት በኋላ የተጣራው ውሃ ይጠራቀምና
ለተጠቃሚዎች ይዳረሳል።
.
▶ስለ surface waterን የማጣራት ሂደቶች ጥቂት የሆነ ገለፃን እንዳደረግንላችሁ ተስፋ
እናደርጋለን ። ርእሱ ሰፊ እንደመሆኑ ዳግመኛ በጥልቀት ለመዳሰስ ቃል እንገባለን✌
.
👇👇👇👇👇
Join for more updates via the link below;
t.me/COTMp
👆👆👆👆👆
⚡ አሁኑኑ Join በማረግ እና ለጓደኛዎ እና ለሚያቁት ሁሉ ሼር ያድርጉ።
.
👉ለዛሬ ደሞ የ ላየኛው የምድር ውሃ (surface water) ለማጣራት የምንጠቀማቸው ዘዴዎች ኣዘጋጅተናል 👇
.
⓵ስክሪኒንግ (screening) - ይህ የመጀመረርያው የማጣራት
ደረጃ ሲሆን በዚህ የማጣራት ዘዴ ውስጥ በውሃው ላይ የሚንሳፈፉ ግዙፍ አካላትን ለምሳሌ የዛፍ ጉቶ ፣ግንድ፣ ቅጠል እና ልዩ ልዩ የፕላስቲክ ተንሳፋፊ ቁሳቁሶች ወደ ዋናው የማጣሪያ ገንዳ እና ስርዓት
እንዳይገቡ ያግዳል ።
.
⓶ማርጋት (Coagulation )፦ በዚህ የማጣራት ደረጃ ላይ
ለአይን እይታ ያነሱ ጥቃቅን
አካላትን (Particle size 10^-7cm የሚሆኑ) በማርጋት እና
የኬሚካል ቻርጃቸውን ኒውትራላይዝ የሚያረግ ኬሚካል በመጨመር እርስ በእርሳቸው
እንዲሳሳቡ ማድረግ ነው ።
ለዚህ የአልሙኒየም ፖሊመሮች (Alum) እና አይረን (Fe+3)
አገልግሎት ላይ ይውላሉ።
እንደ የቁልቋል ተክል ያሉ የተፈጥሮ አርጊዎች (coagulants) መጠቀምም ይቻላል
.
⓷ጉግለት (Flocculation)፦ ይህ እርከን ፤ ማርጋት
(coagulation ) ወቅት የረጉ ጥቃቅን አካላትን እርስ በእርሳቸው ቦንድ እስኪፈጥሩ እና እርስ በእርሳቸው ተጣብቀው እስኪጓግሉ ውሃው በተለያየ ፍጥነት የሚማሰልበት ነው።
ይህ ዘዴ ሜካኒካል ወይም ማኑዋል በሆነ መልኩ ይተገበራል።
.
⓸መዝቀጥ/ማዝቀጥ (sedimentation) ፦ በፍሎኩሌሽን ወቅት የጓጎለው ጥቃቅን አካላት በዚህን የማጣራት ደረጃ እንዲዘቅጡ ይደረጋል ። ይህ ዘዴ የሚተገበረው የሚጣራው የውሃን ፍጥነት በመቀነስ ግራቪቲን ተጠቅሞ እንዲዘቅጥ ማድረግ ነው።
በግራቪቲ ለማዝቀጥ የሚከብዱ እጅግ ጥቃቅን ቆሻሻዎችን በፍሎኩሌሽን ወቅት ስንጠቀማቸው የነበሩ ኬሚካሎችን በመጠቀም እንዲዘቅጡ ይደረጋል።
.
⓹ ማጥራት (filtration ) ፦ በዚህ የማጥራት ደረጃ ከማዝቀጥ
ደረጃ ያለፉ ጥቃቅን ቆሻሻዎችን እጅግ ጥቃቅን ቀዳዳዎች ባሉት አካል (medium ) እንዲያልፍ በማድረግ የድፍረስነቱን መጠን እጅግ መቀነስ ነው።
.
⓺ማከም (Disinfection) ፦ ከላይ በተጠቀሱ የማጣሪያ ሂደቶች የተጣራው ውሃ
(በዋነኛነት ከተለያዩ ህይወት ከሌላቸው ጥቃቅን ቆሻሻዎች)
ለህብረተሰቡ ለአገልግሎት
ከመድረሱ በፊት በዚህ ሂደት (ዲስኢንፌክሽን) ማለፍ አለበት ።
ምክንያቱም ውሃው ለአገልግሎት የሚቀርበው ከተለያዩ በአይን ከማይታዩ በሽታ አምጪ ተህዋስያን ነፃ መሆኑ ሲረጋገጥ ነው ። ዲስኢንፌክሽን ውሃውን በማፍላት ፣ ሚካኒካል
በሆነ መልኩ ፣ ለጨረር በማጋለጥ (radiation ) እንደሁም በኬሚካል ሊከናወን ይችላል።
በሃገራችን በዋነኛነት
ሃሎጅኖችን (ብሮሚን ክሎሪን እና አይኦዲን ) በመጠቀም
ኬሚካል በመጠቀም ውሃን እናክማለን ።
፟
➡ከዚህ ሁሉ የማጣራት ሂደት በኋላ የተጣራው ውሃ ይጠራቀምና
ለተጠቃሚዎች ይዳረሳል።
.
▶ስለ surface waterን የማጣራት ሂደቶች ጥቂት የሆነ ገለፃን እንዳደረግንላችሁ ተስፋ
እናደርጋለን ። ርእሱ ሰፊ እንደመሆኑ ዳግመኛ በጥልቀት ለመዳሰስ ቃል እንገባለን✌
.
👇👇👇👇👇
Join for more updates via the link below;
t.me/COTMp
👆👆👆👆👆
⚡ አሁኑኑ Join በማረግ እና ለጓደኛዎ እና ለሚያቁት ሁሉ ሼር ያድርጉ።
Telegram
ETCONp Discussion
📩ለማነኛውም ሀሳብ እና አስተያየት @Philemona7
✌️ይህ የ @etconp መወያያ ግሩፓቹ ነው።
✋This is discussion group of @ETCONpWORK
.
🔖ማሳሰብያ ...
.
⚡️ግሩፑ ላይ ማነኛውም ከ ኮንስትራክሽን ጉዳዮች ውጪ መለጠፍ በፍፁም አይፈቀድም!
@ETCONpBOT ፃፉልን እናመሰግናለን🙏
✌️ይህ የ @etconp መወያያ ግሩፓቹ ነው።
✋This is discussion group of @ETCONpWORK
.
🔖ማሳሰብያ ...
.
⚡️ግሩፑ ላይ ማነኛውም ከ ኮንስትራክሽን ጉዳዮች ውጪ መለጠፍ በፍፁም አይፈቀድም!
@ETCONpBOT ፃፉልን እናመሰግናለን🙏
Forwarded from Ethio Construction Engineering
👉Load Combination
.
Load Combination - አንድ ፎቅ ላይ የሚመጡ ሎዶችን Analyze ስናደርግ ሁሉም ሎዶች (LL,DL,EQ,WL, etc)
በተመሳሳይ ሰዓት ይከሰታሉ ተብሎ አይታሰብም እንደዛ ቢሆን ኖሮ ለትንንሽ ፎቆች ትልልቅ size ያላቸው Beam, Column እና
Slab ባስፈለገንና Uneconomical በሆንን ነበር፡፡ እንትን ሎድና እንትን ሎድ አንድ ላይ ሲከሰት ወዘተ እያልን Load
Combination እናወጣለን፡፡ ሎዶቹንም በ Factor እናባዛቸዋለን:: Factor ያስፈለገበትም ምክንያት Load
occurrence probability እና በተለያዩ ምክንያቶች የሚፈጠሩ
Load Uncertainties ለማስወገድ ነው፡፡
.
ስንት Load Combination አለ??
.
.
ብዙ ምሁራን በ Load Combination ብዛት ሲወዛገቡ ይታያል፡፡
አንዳንዶች 2 ነው ይላሉ ፤ ሌሎች 7 ነው ይላሉ ፤ ሌሎሎሎች 5
፤ ሌሎሎሎሎሎች 11……..ለማንኛውም ሰባትና ዘጠኝ ናቸው!!!
.
.
ሰባት የሚሆነው Earth Quake እና Wind Loadን እኛ
ካልኩሌት አድርገን ከሁለቱ Govern የሚያደርገውን ከለየን በኋላ
Governing ሎዱን በቁጥር ለሴፍትዌሩ (SAP/Etabs)
ስንሰጠው ሰባት ነው፡፡
.
.
ዘጠኝ የሚሆነው የ Earth Quake ወይም Wind ሎዱን የተለያዩ ፋክተሮች ለሶፍትዌሩ እንሰጠውና እራሱ ሶፍትዌሩ ሎዱን ካልኩሌት አድርጎ አንዲጠቀም ከፈለግን ዘጠኝ Combo እንጠቀማለን፡፡
.
Load Combination - አንድ ፎቅ ላይ የሚመጡ ሎዶችን Analyze ስናደርግ ሁሉም ሎዶች (LL,DL,EQ,WL, etc)
በተመሳሳይ ሰዓት ይከሰታሉ ተብሎ አይታሰብም እንደዛ ቢሆን ኖሮ ለትንንሽ ፎቆች ትልልቅ size ያላቸው Beam, Column እና
Slab ባስፈለገንና Uneconomical በሆንን ነበር፡፡ እንትን ሎድና እንትን ሎድ አንድ ላይ ሲከሰት ወዘተ እያልን Load
Combination እናወጣለን፡፡ ሎዶቹንም በ Factor እናባዛቸዋለን:: Factor ያስፈለገበትም ምክንያት Load
occurrence probability እና በተለያዩ ምክንያቶች የሚፈጠሩ
Load Uncertainties ለማስወገድ ነው፡፡
.
ስንት Load Combination አለ??
.
.
ብዙ ምሁራን በ Load Combination ብዛት ሲወዛገቡ ይታያል፡፡
አንዳንዶች 2 ነው ይላሉ ፤ ሌሎች 7 ነው ይላሉ ፤ ሌሎሎሎች 5
፤ ሌሎሎሎሎሎች 11……..ለማንኛውም ሰባትና ዘጠኝ ናቸው!!!
.
.
ሰባት የሚሆነው Earth Quake እና Wind Loadን እኛ
ካልኩሌት አድርገን ከሁለቱ Govern የሚያደርገውን ከለየን በኋላ
Governing ሎዱን በቁጥር ለሴፍትዌሩ (SAP/Etabs)
ስንሰጠው ሰባት ነው፡፡
.
.
ዘጠኝ የሚሆነው የ Earth Quake ወይም Wind ሎዱን የተለያዩ ፋክተሮች ለሶፍትዌሩ እንሰጠውና እራሱ ሶፍትዌሩ ሎዱን ካልኩሌት አድርጎ አንዲጠቀም ከፈለግን ዘጠኝ Combo እንጠቀማለን፡፡
Forwarded from Ethio Construction Engineering
👉 የትኛው ኢኮኖሚካል ነው ?? => Flat Plate, Waffle, Flat
with Drop or Solid Slab @COTMp
.
.
በጠቅላላው በፍሎር ደረጃ ኢሄኛው የተሻለ ኢኮኖሚካል ነው
አይደለም ለማለት Quantity ካልሰራን ለማወቅ አስቸጋሪ ነው ….
በፓኔል ደረጃ ( ስለአንድ እስላብ ብቻ ) ካወራን ግን EBCS
ሪኮመንድ የሚያረጋቸው የስላብ አይነቶች አሉ ፡፡ ሪኮመንዴሽኑ
100 ፐርሰንት ትክክል ነው ማለት አይደለም - ኢኮኖሚካል ነው
ለማለት ጂኦሜትሪንና የፌሮ ብዛትን ግምት ውስጥ ማስገባት
አለብን - ስለዚህ አሁንም 100 ፐርሰንት እርግጠኛ የምንሆነው
ኳንቲቲ በመስራት ብቻ ነው፡፡ ነገር ግን ኮዱ ባደረገው ጥናት
መሰረት ከኮለን እስከ ኮለን ያለውን ርቀት መሰረት አድርጎ
ኢኮኖሚካል ነው ያለውን የስላብ አይነት አስቀምጡዋል፡፡
እነዚህም፡
.
.
1. Flat Plate - ሎዱ ቀላል ከሆነና ከኮለን ሴንተር እስከ ኮለን
ሴንተር ከ4.5 እስከ 6ሜ ለሆነ ስላብ ኢኮኖሚካል ነው
.
2. Flat Slab With Drop - ከባድ ሎድ ካለና ከሴንተር -
ሴንተር ከ6 እስከ 9ሜ. ለሆነ እስላብ ኢኮኖሚካል ነው፡፡
.
3. Waffle Slab - ለትልቅ እስፓን ከ7.5 – 12ሜ………
ለትልቅ እስፓን ከmoment ይልቅ vertical load ገቨርን
ስለሚያደርግ መሃል ስፓን ላይ ያለውን የስላብ ውፍረት መቀነስ
እንችላለን - ዋፍል ስላብ በመጠቀም ማለት ነው፡፡
.
4. Ribbed Slab -ትልቅ ስፓን ላላቸውና ከቀላል እስከ
መካከለኛ የሆነ ተንቀሳቃሽ ሎድ ላላቸው ፓኔሎች ኢኮኖሚካል
ነው፡፡
.
5. Solid Slab - የስፓኑ ርዝመት በጨመረ ቁጥር ኢኮኖሚካል
አይደለም፡፡ ፍላት ስላቦች ናቸው ኢኮኖሚካል የሚሆኑት
ምክንያቱም የፍላት ስላብ ብረት አቀማመጥ በ Strip ስለሆነ
የፌሮ ብዛት ይቀንሳል::
with Drop or Solid Slab @COTMp
.
.
በጠቅላላው በፍሎር ደረጃ ኢሄኛው የተሻለ ኢኮኖሚካል ነው
አይደለም ለማለት Quantity ካልሰራን ለማወቅ አስቸጋሪ ነው ….
በፓኔል ደረጃ ( ስለአንድ እስላብ ብቻ ) ካወራን ግን EBCS
ሪኮመንድ የሚያረጋቸው የስላብ አይነቶች አሉ ፡፡ ሪኮመንዴሽኑ
100 ፐርሰንት ትክክል ነው ማለት አይደለም - ኢኮኖሚካል ነው
ለማለት ጂኦሜትሪንና የፌሮ ብዛትን ግምት ውስጥ ማስገባት
አለብን - ስለዚህ አሁንም 100 ፐርሰንት እርግጠኛ የምንሆነው
ኳንቲቲ በመስራት ብቻ ነው፡፡ ነገር ግን ኮዱ ባደረገው ጥናት
መሰረት ከኮለን እስከ ኮለን ያለውን ርቀት መሰረት አድርጎ
ኢኮኖሚካል ነው ያለውን የስላብ አይነት አስቀምጡዋል፡፡
እነዚህም፡
.
.
1. Flat Plate - ሎዱ ቀላል ከሆነና ከኮለን ሴንተር እስከ ኮለን
ሴንተር ከ4.5 እስከ 6ሜ ለሆነ ስላብ ኢኮኖሚካል ነው
.
2. Flat Slab With Drop - ከባድ ሎድ ካለና ከሴንተር -
ሴንተር ከ6 እስከ 9ሜ. ለሆነ እስላብ ኢኮኖሚካል ነው፡፡
.
3. Waffle Slab - ለትልቅ እስፓን ከ7.5 – 12ሜ………
ለትልቅ እስፓን ከmoment ይልቅ vertical load ገቨርን
ስለሚያደርግ መሃል ስፓን ላይ ያለውን የስላብ ውፍረት መቀነስ
እንችላለን - ዋፍል ስላብ በመጠቀም ማለት ነው፡፡
.
4. Ribbed Slab -ትልቅ ስፓን ላላቸውና ከቀላል እስከ
መካከለኛ የሆነ ተንቀሳቃሽ ሎድ ላላቸው ፓኔሎች ኢኮኖሚካል
ነው፡፡
.
5. Solid Slab - የስፓኑ ርዝመት በጨመረ ቁጥር ኢኮኖሚካል
አይደለም፡፡ ፍላት ስላቦች ናቸው ኢኮኖሚካል የሚሆኑት
ምክንያቱም የፍላት ስላብ ብረት አቀማመጥ በ Strip ስለሆነ
የፌሮ ብዛት ይቀንሳል::
What is the name of the material placed on the ground surface before pouring any concrete?
Anonymous Quiz
20%
Polyurethane material
51%
Polyethylene sheet
17%
Fabric filter membrane
12%
Fiber glass mesh membrane
It is called 1000 gauge polyethylene sheet.
It is also known by the name plastic sheet, polyfilm, polysheet. It is a plastic sheet made of polymer and ethylene. It serves a lot of purposes in construction. It has various sheet thickness given in gauge . 500 and 1000 gauge are common and are mostly used in construction.
It's primary use is to prevent structural damping and used as vapor barrier memrane in retarding moisture from coming up through concrete into the structure.
In this particular scenario, a 1000 gauge polyethylene sheet is laid underneath the concrete to prevent moisture from being absorbed. No concrete should be poured directly on a ground surface. It protects the reinforced concrete structure as a damproof membrane. ✌👷♂️
@etconp
It is also known by the name plastic sheet, polyfilm, polysheet. It is a plastic sheet made of polymer and ethylene. It serves a lot of purposes in construction. It has various sheet thickness given in gauge . 500 and 1000 gauge are common and are mostly used in construction.
It's primary use is to prevent structural damping and used as vapor barrier memrane in retarding moisture from coming up through concrete into the structure.
In this particular scenario, a 1000 gauge polyethylene sheet is laid underneath the concrete to prevent moisture from being absorbed. No concrete should be poured directly on a ground surface. It protects the reinforced concrete structure as a damproof membrane. ✌👷♂️
@etconp
👍1
Forwarded from Ethio Construction Engineering
👉TYPES OF STAIRS: @COTMp
.
▶Depending upon the various arrangement of steps, stairs can be classified under following categories:
1. STRAIGHT STAIR:
In this stair, all the steps are arranged continuously
along in one direction. One flight may be split into
one or more than one flight by interposing a
landing. This stair can be used where narrow and
long space is available for a staircase such as
entrance, porch etc.
2. DOGGED-LEGGED STAIR:
This stair consists of two straight flights of steps
with direct turns between them. This stair is very
useful where the total width of the stair is just twice
the width of the steps.
3. OPEN NEWEL STAIR:
This type of stair consists of two or more flights
arranging a well or opening between the backward
and forward flights. When all the steps are difficult
to arrange in two flights, a short third flight of 3 to
6 steps may be provided along the direction
perpendicular to the hall. Open newel stair is mostly
adopted in the lift.
4. GEOMETRICAL STAIR:
This is another type of open newel stair where the
open well between the forward and the backward
flight is curved. This stair may contain different
geometrical shape. Here the change in direction is
achieved by using winders.
5. CIRCULAR STAIR:
In this type of stair, all the steps radiate from a
newel or well hole, in the form of winders. The
circular stair is adopted at the back side of a
building to access its various floors.
6. SPIRAL STAIR:
Spiral stair is very similar to a circular stair. It
consists of individual steps or treads, connecting to
a centre column. The overall diameter of the stair
may range from 1 to 2.5 m.
7. QUARTER-TURN STAIR:
The quarter-turn stair can be defined as the stairs
that are turned at 90 degrees with the help of level
landing.
8. BIFURCATED STAIR:
This type of stair is provided in modern public
buildings as well as residential buildings. In this
stair, the flight is so arranged that there is a wide
flight at the start which is sub-divided into narrow
flights at the mid-landing. The narrow flights start
from either side of the mid landing.
.
🚩Join for more Discussion @COTMA
👇👇👇👇👇👇
@COTMA @COTMA @COTMA
.
▶Depending upon the various arrangement of steps, stairs can be classified under following categories:
1. STRAIGHT STAIR:
In this stair, all the steps are arranged continuously
along in one direction. One flight may be split into
one or more than one flight by interposing a
landing. This stair can be used where narrow and
long space is available for a staircase such as
entrance, porch etc.
2. DOGGED-LEGGED STAIR:
This stair consists of two straight flights of steps
with direct turns between them. This stair is very
useful where the total width of the stair is just twice
the width of the steps.
3. OPEN NEWEL STAIR:
This type of stair consists of two or more flights
arranging a well or opening between the backward
and forward flights. When all the steps are difficult
to arrange in two flights, a short third flight of 3 to
6 steps may be provided along the direction
perpendicular to the hall. Open newel stair is mostly
adopted in the lift.
4. GEOMETRICAL STAIR:
This is another type of open newel stair where the
open well between the forward and the backward
flight is curved. This stair may contain different
geometrical shape. Here the change in direction is
achieved by using winders.
5. CIRCULAR STAIR:
In this type of stair, all the steps radiate from a
newel or well hole, in the form of winders. The
circular stair is adopted at the back side of a
building to access its various floors.
6. SPIRAL STAIR:
Spiral stair is very similar to a circular stair. It
consists of individual steps or treads, connecting to
a centre column. The overall diameter of the stair
may range from 1 to 2.5 m.
7. QUARTER-TURN STAIR:
The quarter-turn stair can be defined as the stairs
that are turned at 90 degrees with the help of level
landing.
8. BIFURCATED STAIR:
This type of stair is provided in modern public
buildings as well as residential buildings. In this
stair, the flight is so arranged that there is a wide
flight at the start which is sub-divided into narrow
flights at the mid-landing. The narrow flights start
from either side of the mid landing.
.
🚩Join for more Discussion @COTMA
👇👇👇👇👇👇
@COTMA @COTMA @COTMA
👍1
Forwarded from Ethio Construction Engineering
👉BASICS OF CRACKING PROBLEMS: @COTMp
.
▶The subject “ CRACKS “ or “ CRACKING “ in
concrete is indeed much debated. However, there is
inadequate clarity as to the reason for cracking and
what mey be done to limit its occurrence or
eliminate it altogether.
The phenomenon of the appearance of cracks in
concrete is often a subject that raises several
questions. Either at the initial stage or with time,
cracks may appear in a concrete structure. It should
first of all be accepted that cracks of some type or
other are inevitable in any concrete. They can be
minimized to a large extent by proper practices.
Cracks may be big or small, structural or non-
structural. All of them can be a nuisance by way of
either marring the appearance or function as a
passage for atmospheric polluting gases and
moisture to either the body of concrete and causes
distress.
Cracks in the concrete structure do not always
mean that the structure is not useable. As cracking
of concrete is inherent, what really matters is the
type of structure and the nature of cracking. Cracks
that are acceptable for building structures may not
be acceptable for water relating structures.
Considering that cracking xan never be completely
eliminated, it is necessary to be aware of the
causes, evaluation and the methods of repair
whoever required.
CRACKS
Cracks are generally of towtypes : Structural and
non-structural. Cracks can occur in hardened or
unhardened concrete.
STRUCTURAL CRACKS
It is fundamental that hardened reinforced concrete
cracks in the tensile zone when subjected to
externally imposed structural loads. By means of
appropriate design and detailing technique, these
cracks can be limited to acceptable levels in terms
of structural integrity and aesthetics.
NON_STRUCTURAL CRACKS
Concrete is also liable to crack in both the plastic
and hardened states due to the nature of its
constituent materials. These intrinsic cracks are as
inevitable as structural cracks. Ti is often possible
to predict when intrinsic cracks are likely and to
limit them to acceptable levels by means of good
design and/or proper construction techniques.
DORMANT AND LIVE CRACKS:
Cracks caused by shrinkage, temperature gradient
due to hydration and alkali silica reaction ( ASR )
are less dangerous the cracks caused by thermal
expansion and loads. This is because shrinkage
and hydration temperature gradient result in
dormant cracks ( where the width does not vary
with time) and other mechanisms result in live
cracks (where the width increases with time
Dormant cracks, especially narrow ones, are more
likely to undergo autogenous healing and
realkalisation. The crack may heal owing to
following conditions:
• carbon dioxide diffusing into the crack leading to
carbonation of the calcium hydroxide and
precipitation of calcium carbonate.
• Cement hydration due to presence of moisture.
• Hydration diffusing from the bulk concrete into the
heaked zone thereby increasing the pH in that area.
Live cracks are more likely than domant ones. They
result in collection of debris at the base owing to
movement of the sides on the cracks. This can
impede temporarily the passage of depassivating
substances to the reinforcements. However,
autodeneous healing is unlikely with live cracks.
CAUSES OF CRACKING:
Cracking will occur whenever the applied strain
exceeds the tensile strain capacity of the concrete.
The tensile strain capacity of concrete varies with
age and with
Age at which cracks may occur.
Cracks can appear at any time. The age which
some typical can occur are given in the Table.
TABLE – AGE AT WHICH CRACKS MAY APPEAR:
Sr. no. types of cracks Age
1. plastic shrinkage First few minutes or hours after
concreting .
2. plastic settlement First few minutes or hours
after concreting.
3. due to corrosion After one year or many years.
4. due to loads After loads are imposed and the
time duration of loading
5. due to weight Just after formwork support are
removed.👇👇👇
.
▶The subject “ CRACKS “ or “ CRACKING “ in
concrete is indeed much debated. However, there is
inadequate clarity as to the reason for cracking and
what mey be done to limit its occurrence or
eliminate it altogether.
The phenomenon of the appearance of cracks in
concrete is often a subject that raises several
questions. Either at the initial stage or with time,
cracks may appear in a concrete structure. It should
first of all be accepted that cracks of some type or
other are inevitable in any concrete. They can be
minimized to a large extent by proper practices.
Cracks may be big or small, structural or non-
structural. All of them can be a nuisance by way of
either marring the appearance or function as a
passage for atmospheric polluting gases and
moisture to either the body of concrete and causes
distress.
Cracks in the concrete structure do not always
mean that the structure is not useable. As cracking
of concrete is inherent, what really matters is the
type of structure and the nature of cracking. Cracks
that are acceptable for building structures may not
be acceptable for water relating structures.
Considering that cracking xan never be completely
eliminated, it is necessary to be aware of the
causes, evaluation and the methods of repair
whoever required.
CRACKS
Cracks are generally of towtypes : Structural and
non-structural. Cracks can occur in hardened or
unhardened concrete.
STRUCTURAL CRACKS
It is fundamental that hardened reinforced concrete
cracks in the tensile zone when subjected to
externally imposed structural loads. By means of
appropriate design and detailing technique, these
cracks can be limited to acceptable levels in terms
of structural integrity and aesthetics.
NON_STRUCTURAL CRACKS
Concrete is also liable to crack in both the plastic
and hardened states due to the nature of its
constituent materials. These intrinsic cracks are as
inevitable as structural cracks. Ti is often possible
to predict when intrinsic cracks are likely and to
limit them to acceptable levels by means of good
design and/or proper construction techniques.
DORMANT AND LIVE CRACKS:
Cracks caused by shrinkage, temperature gradient
due to hydration and alkali silica reaction ( ASR )
are less dangerous the cracks caused by thermal
expansion and loads. This is because shrinkage
and hydration temperature gradient result in
dormant cracks ( where the width does not vary
with time) and other mechanisms result in live
cracks (where the width increases with time
Dormant cracks, especially narrow ones, are more
likely to undergo autogenous healing and
realkalisation. The crack may heal owing to
following conditions:
• carbon dioxide diffusing into the crack leading to
carbonation of the calcium hydroxide and
precipitation of calcium carbonate.
• Cement hydration due to presence of moisture.
• Hydration diffusing from the bulk concrete into the
heaked zone thereby increasing the pH in that area.
Live cracks are more likely than domant ones. They
result in collection of debris at the base owing to
movement of the sides on the cracks. This can
impede temporarily the passage of depassivating
substances to the reinforcements. However,
autodeneous healing is unlikely with live cracks.
CAUSES OF CRACKING:
Cracking will occur whenever the applied strain
exceeds the tensile strain capacity of the concrete.
The tensile strain capacity of concrete varies with
age and with
Age at which cracks may occur.
Cracks can appear at any time. The age which
some typical can occur are given in the Table.
TABLE – AGE AT WHICH CRACKS MAY APPEAR:
Sr. no. types of cracks Age
1. plastic shrinkage First few minutes or hours after
concreting .
2. plastic settlement First few minutes or hours
after concreting.
3. due to corrosion After one year or many years.
4. due to loads After loads are imposed and the
time duration of loading
5. due to weight Just after formwork support are
removed.👇👇👇
👍1
Forwarded from Ethio Construction Engineering
6. due to chemical changes in hardened
concrete After one or many years depending in
chemical attack from outside (sulphate ) Or
chemical reaction from within (ASR)
.
▶CRITICAL CRACK WIDTH: The most common reasons for controlling crack
width are following:
APPERANCE : Unsightly cracking should be avoid
since it may cause concern to the occupants of the external structure.
Ti may also contribute to
unsightly staining on exposed external surfaces,
where salts and rust are washed out from the crack.
DURABILITY: Excessively wide cracks may lead to
corrosion of the reinforcement which in turn may lead to spalling of concrete due to the expansive nature of the corrosion process.
WATER-TIGHTNESS: This is of importance in water
retaining structures.
In particular instances there may be other reasons for controlling cracking in addition to the three reasons cited above.
Crack width is, generally, to be taken to mean the
measurable width of a crack at the surface of
concrete. Crack width limitation is important from durability considerations. Most structural codes
prescribe maximum allowed crack widths.
Codes normally consider cracking caused by
external imposed conditions such as live loading
and provide formula for calculating the crack width
in the design phase. Mainly bending and tension or
bending and axial load are considered. The
direction of such cracks is perpendicular to the
direction of the main reinforcement. Plastic
shrinkage cracks follow the line of reinforcement.
According to IS: 456-2000 the surface of the width
of the cracks should not in general exceeds o.3 mm
in members where cracking is not harmful and does
not have any serious effect either on the
preservation of reinforceing steel or on the durability
of the structures.
In members, where cracking of the tensile zone is
harmful either because they are moisture or in
contact with soil or groundwater, an upper limlt of
0.2 mm is suggested.
For aggressive conditions the surface width of
cracks should not generally exceed 0.1 mm. The
crack width conditions the surface width of cracks
should not be generally exceed 0.1 mm. The crack
width is measured at the surface for the above
purposes. However some other codes specify the
width at points near the reinforcement.
.
🚩Share Share Share
concrete After one or many years depending in
chemical attack from outside (sulphate ) Or
chemical reaction from within (ASR)
.
▶CRITICAL CRACK WIDTH: The most common reasons for controlling crack
width are following:
APPERANCE : Unsightly cracking should be avoid
since it may cause concern to the occupants of the external structure.
Ti may also contribute to
unsightly staining on exposed external surfaces,
where salts and rust are washed out from the crack.
DURABILITY: Excessively wide cracks may lead to
corrosion of the reinforcement which in turn may lead to spalling of concrete due to the expansive nature of the corrosion process.
WATER-TIGHTNESS: This is of importance in water
retaining structures.
In particular instances there may be other reasons for controlling cracking in addition to the three reasons cited above.
Crack width is, generally, to be taken to mean the
measurable width of a crack at the surface of
concrete. Crack width limitation is important from durability considerations. Most structural codes
prescribe maximum allowed crack widths.
Codes normally consider cracking caused by
external imposed conditions such as live loading
and provide formula for calculating the crack width
in the design phase. Mainly bending and tension or
bending and axial load are considered. The
direction of such cracks is perpendicular to the
direction of the main reinforcement. Plastic
shrinkage cracks follow the line of reinforcement.
According to IS: 456-2000 the surface of the width
of the cracks should not in general exceeds o.3 mm
in members where cracking is not harmful and does
not have any serious effect either on the
preservation of reinforceing steel or on the durability
of the structures.
In members, where cracking of the tensile zone is
harmful either because they are moisture or in
contact with soil or groundwater, an upper limlt of
0.2 mm is suggested.
For aggressive conditions the surface width of
cracks should not generally exceed 0.1 mm. The
crack width conditions the surface width of cracks
should not be generally exceed 0.1 mm. The crack
width is measured at the surface for the above
purposes. However some other codes specify the
width at points near the reinforcement.
.