It is called a neck column (column neck)

Neck column refers to the substructure column located between foundation structure and Grade beam.

The same waterproofing and damp proofing done for the foundation should also be done to the neck column.

Make no mistake, some individuals use foundation column or footing column to describe this column. But in most cases neck column is widely used by scholars so it is important not to be confused when hearing the word neck column.

Floating columns are vertical members which rest on the beam which is not directly connected to foundation structure.

I will wrap up my journal regarding the first phases of building construction. Roughly this is what a substructure work looks like.

Attached below is the typical section of an isolated footing. 25cm fill material,1000 gauge polyethylene sheet, blinding PCC, bitumen waterproofing and the RC structure is shown.

✌👷‍♂️.
👉BASICS OF CRACKING PROBLEMS: @COTMp
.
▶The subject “ CRACKS “ or “ CRACKING “ in
concrete is indeed much debated. However, there is
inadequate clarity as to the reason for cracking and what may be done to limit its occurrence or
eliminate it altogether.
The phenomenon of the appearance of cracks in
concrete is often a subject that raises several
questions. Either at the initial stage or with time,
cracks may appear in a concrete structure. It should first of all be accepted that cracks of some type or other are inevitable in any concrete. They can be minimized to a large extent by proper practices.
*Cracks may be big or small, structural or non-
structural. All of them can be a nuisance by way of
either marring the appearance or function as a passage for atmospheric polluting gases and
moisture to either the body of concrete and causes
distress.
*Cracks in the concrete structure do not always
mean that the structure is not usable. As cracking
of concrete is inherent, what really matters is the
type of structure and the nature of cracking. Cracks
that are acceptable for building structures may not be acceptable for water relating structures.
Considering that cracking can never be completely
eliminated, it is necessary to be aware of the
causes, evaluation and the methods of repair
whoever required.
CRACKS Cracks are generally of tow types : Structural and nonstructural
*Cracks can occur in hardened or unhardened concrete.
*STRUCTURAL CRACKS
It is fundamental that hardened reinforced concrete cracks in the tensile zone when subjected to externally imposed structural loads. By means of appropriate design and detailing technique, these cracks can be limited to acceptable levels in terms
of structural integrity and aesthetics.
*NON_STRUCTURAL CRACKS
**Concrete is also liable to crack in both the plastic
and hardened states due to the nature of its
constituent materials. These intrinsic cracks are as inevitable as structural cracks. It is often possible
to predict when intrinsic cracks are likely and to
limit them to acceptable levels by means of good
design and/or proper construction techniques.
*DORMANT AND LIVE CRACKS:
Cracks caused by shrinkage, temperature gradient due to hydration and alkali silica reaction ( ASR ) are less dangerous the cracks caused by thermal expansion and loads. This is because shrinkage and hydration temperature gradient result in dormant cracks ( where the width does not vary with time) and other mechanisms result in live
cracks (where the width increases with time
Dormant cracks, especially narrow ones, are more
likely to undergo auto genius healing and
realkalisation. The crack may heal owing to
following conditions:
• carbon dioxide diffusing into the crack leading to
carbonation of the calcium hydroxide and
precipitation of calcium carbonate.
• Cement hydration due to presence of moisture.
• Hydration diffusing from the bulk concrete into the
heaked zone thereby increasing the pH in that area.
Live cracks are more likely than domant ones. They
result in collection of debris at the base owing to movement of the sides on the cracks. This can
impede temporarily the passage of depassivating
substances to the reinforcements. However,
autodeneous healing is unlikely with live cracks.
▶CAUSES OF CRACKING:
Cracking will occur whenever the applied strain exceeds the tensile strain capacity of the concrete.
*The tensile strain capacity of concrete varies with age and with
Age at which cracks may occur.
*Cracks can appear at any time. The age which
some typical can occur are given in the Table.
▶TABLE – AGE AT WHICH CRACKS MAY APPEAR:
*Sr. no. types of cracks Age
1. plastic shrinkage First few minutes or hours after
concreting .
2. plastic settlement First few minutes or hours
after concreting.
3. due to corrosion After one year or many years.
4. due to loads After loads are imposed and the
time duration of loading.
👇👇👇👇👇
👆👆👆👆👆
🇪 🇫 🇫 🇱 🇴 🇷 🇪 🇸 🇨 🇪 🇳 🇨 🇪

Efflorescence is one type of defect found on plaster surface. Efflorescence is the whitish crystalline substance which appears on the surface of walls due to presence of soluble salts, such as suphates of sodium, calcium and magnesium.

WHY EFFLORESCENCE HAPPENS ON PLASTER SURFACE?

Presence of salts in the lime, cement, sand, bricks and sometimes even in water used in construction work are the cause of efflorescence on plaster surface. After completion of plaster work and when it becomes completely dry; the soluble salts dissolved by moisture are drawn to the surface through pores. These soluble salts absorbs moisture from atmosphere and on drying, they get deposited in patches in form of white crystalline substance. The surface gets disfigured by ugly damp patches of efflorescence. This defect gradually disintegrates the structure. It is normally of temporary in nature as it disappears during wet weather and reappears during dry weather.

HOW TO RECTIFY EFFLORESCENCE OR WHAT ARE THE REMEDIES?

👉Efflorescent salts cannot be removed by washing with water as it may carry some of the salts back into the pore.

👉Dry brushing of the growth as it appears on the surface is one of remedies.

👉 The treatment of an old wall with silicon solution will frequently stop the efflorescence as the liquid blocks the passage for movement of moisture.

👉 When efflorescence is due to the rising of salt solutions through capillary action from subsoil; the only remedy is to provide bitumen or metallic seals in the walls above the ground level so that an effective barrier to the capillary action is created.

👉 In case of brickwork, the salt can be removed with a solution of zinc sulphate and water. The surface is brushed off when dry.

@etconp
👍2
Buckling types

#structure

@etconp
A. 1️⃣
B. 2️⃣
C. 3️⃣
D. 4️⃣

#stair
ለጓደኞቻችው ይህን Channel በማጋራት ቤተሰብ እናፍራ
@etconp

Facebook:- https://www.facebook.com/etconp/
❤1
Ethio Construction Engineering via @like
A. 1️⃣ B. 2️⃣ C. 3️⃣ D. 4️⃣ #stair ለጓደኞቻችው ይህን Channel በማጋራት ቤተሰብ እናፍራ @etconp Facebook:- https://www.facebook.com/etconp/
The answer for this question is

2R + T = 60

The answer is A. 1️⃣


@etconp
Forwarded from Ethio Construction Engineering (Selman💯®©)
👉ዛሬ ደሞ ስለ Load Combination በ ኣዲሱ የ EBCS ኮድ ኣብረን እንይ
.
Combo 1= DL + LL
Combo 2= 1.35DL + 1.5LL
Combo 3= DL + 0.3LL + EQx
Combo 4= DL + 0.3LL - EQx
Combo 5= DL + 0.3LL + EQy
Combo 6= DL + 0.3LL - EQy
Combo 7= max( Combo 2 up to 6)
.
.
ሁሌ ግን ኢሄ ነው ማለት አይደለም፡፡ ለምሳሌ 0.3LL የሚለው
ህንፃውን የምንጠቀመው ለDomestic/residential purpose
ከሆነ ነው፡፡ Shop ከሆነ 0.6LL storage ከሆነ ደሞ 0.8LL
ይሆናል፡፡ ከዚህም በተጨማሪ ሁሉም ፎርሙላ ላይ የተለያዩ
ኮንዲሽኖች ስላሉ እነሱን ማየት ያስፈልጋል፡፡ መገኛቸውም EBCS
EN 1990: 2014 ከ Equation 6.9 እስከ 6.16 ነው፡፡

ፎርሙላዎቹ ውስጥ የሚገቡትን variable ለማግኘት ደሞ
check the Annex part እዩት።
.
combination ሰባት ነው ዘጠኝ ነው ስላልኩት ደሞ ብዙዎች
Earth Quakeም እያለ በሁለትና በሶስት Combination ሲሰሩ
ስላየው ነው፡፡ እንጂ ግዴታ 7 ወይ ምናምን መሆን የለበትም፡፡
ለምሳሌ Serviceability ብቻ ኮንሲደር ካደረግን አንድ ኮምቦ //
ማለትም DL+LL// ሊበቃ ይችላል፡፡ ፅሁፉ ግልፅ ስላልሆነና
ወዳልሆነ አቅጣጫ እንዳይወሰድ አንስቼዋለው፡፡
.
👉ለተጨማሜ የ ኮንስትራክሽን እውቀቶች...
🚩 እዚህ ይጫኑ
👇👇👇👇👇
@COTMp
@COTMp
👍1👌1
What is the name of this shuttering equipment??
Anonymous Quiz
23%
Flange clamp
25%
Tie rod
37%
Props jack
15%
Ledger