👉Today Tip @ETCONp
.
➡ለዛሬ ሙሉ እና ጥልቅ የ FIDIC ዶክመንት ይዘን ቀርበናል።
.
🅾አሁኑኑ Join በማረግ እና ለጓደኛዎ እና ለሚያቁት ሁሉ ሼር ያድርጉ።
፡
👉Today Tip @ETCONp
.
➡ለዛሬ ሙሉ እና ጥልቅ የ FIDIC ዶክመንት ይዘን ቀርበናል።
.
🅾አሁኑኑ Join በማረግ እና ለጓደኛዎ እና ለሚያቁት ሁሉ ሼር ያድርጉ።
👉በአዳማ ሳይንስና ቴክኖሎጂ ዩኒቨርሲቲ ከዛሬ ጀምሮ ለአራት ተከታታይ ቀናት የሚቆይ የአርክቴክቸራል ኤግዚቢሽን በ ARCH STUDIO - 1 እየተካሄደ እንደሆነ የ ቻናላችን ቤተሰቦች ነግረውናል፡፡
.
▶️ተጨማሪ የፎቶ መረጃዎች @ETCONp_Bot ኣድርሱን መልሰን እናቀርባለን፡፡
.
▶️ተጨማሪ የፎቶ መረጃዎች @ETCONp_Bot ኣድርሱን መልሰን እናቀርባለን፡፡
👍1
👉Concrete Cover Distance for Reinforcement Bar @ETCONp
፡
▶️The reinforcement must be fixed with appropriate accuracy in the position specified by the designer to ensure proper structural performance, durability and fire resistance. *Insufficient cover can result in corrosion of the reinforcement, leading to cracking and spalling of the concrete and eventually, if left unchecked, to a reduction in the cross-sectional area of the reinforcement and in the strength of the structure. The cover must also be sufficient to provide the required degree of fire resistance. Too little cover reduces the fire resistance; too much, unless precautionary measures are taken, can make the structure vulnerable to spalling, which again reduces the fi re resistance. Incorrect positioning of the reinforcement can seriously reduce the load-carrying capacity of the structural member.
*Unless otherwise specified, the concrete cover to the reinforcement should be within the following permissible deviations from the dimensions specified in BS 8110:
:
*Bars up to 12 mm diameter: +5mm –5mm
*Bars over 12 mm up to 25 mm: +10 mm –5mm
*Bars over 25 mm: +15 mm –5mm
:
▶️At each end of reinforcing bar, net less that 25 mm or less than twice the diameter of the bar.
*For a longitudinal reinforcing bar in a column, not less than 40 mm not less than the diameter of such bar.
*In case of columns of minimum dimension of 20 cm or under, whose reinforcing bards do no not exceed 12 mm a cover of 25 mm to be used.
*For longitudinal reinforcing bars in a beam, not less than 30 mm or less than the diameter of the bar.
*For tensile, compressive shear or other reinforcements in a slab or wall not less than 15 mm, not less that the diameter of such bar.
*For any other reinforcement not less than 15 mm, not less than the diameter of such bar.
*For footings and other principal structural members in which the concrete is deposited directly against the ground, cover to the bottom reinforcement shall be 75 mm. If concrete is poured on a layer of lean concrete, the bottom cover maybe reduced to 50 mm.
*For concrete surfaces exposed to the weather or the ground after removal of forms, such as retaining walls, grade beams, footing sides and top etc. not less than 50 mm.
*Increased cover thickness shall be provided as indicated on the drawings, for surfaces exposed to the action of harmful chemicals (or exposed to earth contaminated by such chemicals), acid, alkali, saline atmosphere, sulphorone, smoke etc.
*For liquid retaining structures, the minimum cover to all steel shall be 40 mm or the diameter of the main bar, whichever is greater. In the presence of sea water and oils and waters of a corrosive character the covers, shall be increased by 10 mm.
Protection to reinforcement in case of concrete exposed to harmful surroundings may also be given by providing a dense impermeable concrete with approved protective coatings. In such a case the extra cover mentioned in (b) & (i) above may be reduced.
:
▶️The correct cover shall be maintained by cement mortar cubes (blocks) or other approved means. Reinforcements for footings, grade beams and slabs on a sub-grade shall be supported on re-cast concrete blocks as approved by EIC.
*The use of pebbles or stones shall not be permitted.
:
https://t.me/COTMp
፡
▶️The reinforcement must be fixed with appropriate accuracy in the position specified by the designer to ensure proper structural performance, durability and fire resistance. *Insufficient cover can result in corrosion of the reinforcement, leading to cracking and spalling of the concrete and eventually, if left unchecked, to a reduction in the cross-sectional area of the reinforcement and in the strength of the structure. The cover must also be sufficient to provide the required degree of fire resistance. Too little cover reduces the fire resistance; too much, unless precautionary measures are taken, can make the structure vulnerable to spalling, which again reduces the fi re resistance. Incorrect positioning of the reinforcement can seriously reduce the load-carrying capacity of the structural member.
*Unless otherwise specified, the concrete cover to the reinforcement should be within the following permissible deviations from the dimensions specified in BS 8110:
:
*Bars up to 12 mm diameter: +5mm –5mm
*Bars over 12 mm up to 25 mm: +10 mm –5mm
*Bars over 25 mm: +15 mm –5mm
:
▶️At each end of reinforcing bar, net less that 25 mm or less than twice the diameter of the bar.
*For a longitudinal reinforcing bar in a column, not less than 40 mm not less than the diameter of such bar.
*In case of columns of minimum dimension of 20 cm or under, whose reinforcing bards do no not exceed 12 mm a cover of 25 mm to be used.
*For longitudinal reinforcing bars in a beam, not less than 30 mm or less than the diameter of the bar.
*For tensile, compressive shear or other reinforcements in a slab or wall not less than 15 mm, not less that the diameter of such bar.
*For any other reinforcement not less than 15 mm, not less than the diameter of such bar.
*For footings and other principal structural members in which the concrete is deposited directly against the ground, cover to the bottom reinforcement shall be 75 mm. If concrete is poured on a layer of lean concrete, the bottom cover maybe reduced to 50 mm.
*For concrete surfaces exposed to the weather or the ground after removal of forms, such as retaining walls, grade beams, footing sides and top etc. not less than 50 mm.
*Increased cover thickness shall be provided as indicated on the drawings, for surfaces exposed to the action of harmful chemicals (or exposed to earth contaminated by such chemicals), acid, alkali, saline atmosphere, sulphorone, smoke etc.
*For liquid retaining structures, the minimum cover to all steel shall be 40 mm or the diameter of the main bar, whichever is greater. In the presence of sea water and oils and waters of a corrosive character the covers, shall be increased by 10 mm.
Protection to reinforcement in case of concrete exposed to harmful surroundings may also be given by providing a dense impermeable concrete with approved protective coatings. In such a case the extra cover mentioned in (b) & (i) above may be reduced.
:
▶️The correct cover shall be maintained by cement mortar cubes (blocks) or other approved means. Reinforcements for footings, grade beams and slabs on a sub-grade shall be supported on re-cast concrete blocks as approved by EIC.
*The use of pebbles or stones shall not be permitted.
:
https://t.me/COTMp
Telegram
ETCONp Discussion
📩ለማነኛውም ሀሳብ እና አስተያየት @Philemona7
✌️ይህ የ @etconp መወያያ ግሩፓቹ ነው።
✋This is discussion group of @ETCONpWORK
.
🔖ማሳሰብያ ...
.
⚡️ግሩፑ ላይ ማነኛውም ከ ኮንስትራክሽን ጉዳዮች ውጪ መለጠፍ በፍፁም አይፈቀድም!
@ETCONpBOT ፃፉልን እናመሰግናለን🙏
✌️ይህ የ @etconp መወያያ ግሩፓቹ ነው።
✋This is discussion group of @ETCONpWORK
.
🔖ማሳሰብያ ...
.
⚡️ግሩፑ ላይ ማነኛውም ከ ኮንስትራክሽን ጉዳዮች ውጪ መለጠፍ በፍፁም አይፈቀድም!
@ETCONpBOT ፃፉልን እናመሰግናለን🙏
Majestic hotel in Punta del Este, Departamento de Maldonado Uruguay 🇺🇾
ውብ ምሽት ተመኘን
كنا نتمنى أمسية جميلة
我們希望有一個美麗的夜晚
हमने एक खूबसूरत शाम की कामना की
We wished a beautiful evening
Мы пожелали прекрасного вечера
@ETCONp
ውብ ምሽት ተመኘን
كنا نتمنى أمسية جميلة
我們希望有一個美麗的夜晚
हमने एक खूबसूरत शाम की कामना की
We wished a beautiful evening
Мы пожелали прекрасного вечера
@ETCONp
This media is not supported in your browser
VIEW IN TELEGRAM
Why did it fail? We need valid reason
👉PROPERTIES OF PORTLAND CEMENT @COTMp
.
▶️(i) Chemical properties: Portland cement consists of the following chemical compounds:
(a) Tricalcium silicate 3 CaO.SiO2 (C3S) 40%
(b) Dicalcium silicate 2CaO.SiO2 (C2S) 30%
(c) Tricalcium aluminate 3CaO.Al2O3 (C3A) 11%
(d) Tetracalcium aluminate 4CaO.Al2O3.Fe2O3 (C3AF) 11%
There may be small quantities of impurities present such as calcium oxide (CaO) and magnesium oxide (MgO). When water is added to cement, C3A is the first to react and cause initial set. It generates great amount of heat. C3S hydrates early and develops strength in the first 28 days. It also generates heat. C2S is the next to hydrate. It hydrates slowly and is responsible for increase in ultimate strength. C4AF is comparatively inactive compound.
.
▶️(ii) Physical properties:
The following physical properties should be checked before selecting a portland cement for the civil engineering works. IS 269–1967 specifies the method of testing and prescribes the limits:
(a) Fineness (b) Setting time
(c) Soundness (d) Crushing strength.
(a) Fineness:
.
*It is measured in terms of percentage of weight retained after sieving the cement through 90 micron sieve or by surface area of cement in square centimeters per gramme of cement. According to IS code specification weight retained on the sieve should not be more than 10 per cent. In terms of specific surface should not be less than 2250 cm2/gm.
(b) Setting time:
A period of 30 minutes as minimum setting time for initial setting and a maximum period of 600 minutes as maximum setting time is specified by IS code, provided the tests are conducted as per the procedure prescribed by IS 269-1967.
.
(c) Soundness:
Once the concrete has hardened it is necessary to ensure that no volumetric changes takes place. The cement is said to be unsound, if it exhibits volumetric instability after hardening. IS code recommends test with Le Chatelier mould for testing this property. At the end of the test, the indicator of Le Chatelier mould should not expand by more than 10 mm.
***(a) Crushing strength:
For this mortar cubes are made with standard sand and tested in compression testing machine as per the specification of IS code. The minimum strength specified is 16 N/mm2 after 3 days and 22 N/mm2 after 7 days of curing.
:
http://t.me/ETCONp
.
▶️(i) Chemical properties: Portland cement consists of the following chemical compounds:
(a) Tricalcium silicate 3 CaO.SiO2 (C3S) 40%
(b) Dicalcium silicate 2CaO.SiO2 (C2S) 30%
(c) Tricalcium aluminate 3CaO.Al2O3 (C3A) 11%
(d) Tetracalcium aluminate 4CaO.Al2O3.Fe2O3 (C3AF) 11%
There may be small quantities of impurities present such as calcium oxide (CaO) and magnesium oxide (MgO). When water is added to cement, C3A is the first to react and cause initial set. It generates great amount of heat. C3S hydrates early and develops strength in the first 28 days. It also generates heat. C2S is the next to hydrate. It hydrates slowly and is responsible for increase in ultimate strength. C4AF is comparatively inactive compound.
.
▶️(ii) Physical properties:
The following physical properties should be checked before selecting a portland cement for the civil engineering works. IS 269–1967 specifies the method of testing and prescribes the limits:
(a) Fineness (b) Setting time
(c) Soundness (d) Crushing strength.
(a) Fineness:
.
*It is measured in terms of percentage of weight retained after sieving the cement through 90 micron sieve or by surface area of cement in square centimeters per gramme of cement. According to IS code specification weight retained on the sieve should not be more than 10 per cent. In terms of specific surface should not be less than 2250 cm2/gm.
(b) Setting time:
A period of 30 minutes as minimum setting time for initial setting and a maximum period of 600 minutes as maximum setting time is specified by IS code, provided the tests are conducted as per the procedure prescribed by IS 269-1967.
.
(c) Soundness:
Once the concrete has hardened it is necessary to ensure that no volumetric changes takes place. The cement is said to be unsound, if it exhibits volumetric instability after hardening. IS code recommends test with Le Chatelier mould for testing this property. At the end of the test, the indicator of Le Chatelier mould should not expand by more than 10 mm.
***(a) Crushing strength:
For this mortar cubes are made with standard sand and tested in compression testing machine as per the specification of IS code. The minimum strength specified is 16 N/mm2 after 3 days and 22 N/mm2 after 7 days of curing.
:
http://t.me/ETCONp
Telegram
Ethio Construction Engineering
🔨 World Construction Engineering
Latest updates, tips, and tutorials on building, civil engineering, and construction in World.
Learn, build, and grow with us!
📨 @Philemona7 Or @ETCONpBOT
For Ad:- https://telega.io/c/etconp
Latest updates, tips, and tutorials on building, civil engineering, and construction in World.
Learn, build, and grow with us!
📨 @Philemona7 Or @ETCONpBOT
For Ad:- https://telega.io/c/etconp
👉ይቺ ናት ኢትዮጵያ ይቺ ናት ሀገሬ @ETCONp
:
▶️ኢትዮጵያ ሀገራችንን በበጎ ስራ እናገልግል የምህንድስና ሙያን ወደ ከፍታው እንመልስ!!
፡
🙏"ፈጣሪ ኢትዮጵያ እና ህዝቦቿን አብዝቶ ይባርክ!!"🙏
:
👇👇👇👇👇👇👇👇
:
▶️ኢትዮጵያ ሀገራችንን በበጎ ስራ እናገልግል የምህንድስና ሙያን ወደ ከፍታው እንመልስ!!
፡
🙏"ፈጣሪ ኢትዮጵያ እና ህዝቦቿን አብዝቶ ይባርክ!!"🙏
:
👇👇👇👇👇👇👇👇